Kono, Masaru; Clague, David A; Larson, Edwin E (1980): (Table 2) Reflection microscopy of Fe-Ti oxides at DSDP Hole 55-432A [dataset]. PANGAEA, https://doi.org/10.1594/PANGAEA.823365, In supplement to: Kono, M et al. (1980): Fe-Ti oxide mineralogy of DSDP Leg 55 basalts. In: Jackson, ED; Koisumi, I; et al., (eds.), Initial Reports of the Deep Sea Drilling Project (U.S. Govt. Printing Office), 55, 639-652, https://doi.org/10.2973/dsdp.proc.55.126.1980

Always quote citation above when using data! You can download the citation in several formats below.

RIS CitationBibTeX CitationShow MapGoogle Earth

Project(s):
Coverage:
Latitude: 41.333800 * Longitude: 170.379000
Date/Time Start: 1977-08-06T00:00:00 * Date/Time End: 1977-08-06T00:00:00
Minimum Elevation: -1310.0 m * Maximum Elevation: -1310.0 m
Event(s):
55-432A * Latitude: 41.333800 * Longitude: 170.379000 * Date/Time: 1977-08-06T00:00:00 * Elevation: -1310.0 m * Penetration: 74 m * Recovery: 16.1 m * Location: North Pacific/TERRACE * Campaign: Leg55 * Basis: Glomar Challenger * Method/Device: Drilling/drill rig (DRILL) * Comment: 5 cores; 38 m cored; 0 m drilled; 42.4 % recovery
Comment:
+++ = abundant, ++ = common, + = present, - = absent.
Parameter(s):
#NameShort NameUnitPrincipal InvestigatorMethod/DeviceComment
1Sample code/labelSample labelKono, MasaruDSDP/ODP/IODP sample designation
2UnitUnitKono, MasaruFlow unit number and type of rock: A, alkalic basalts, T, tholeiites
3Curie temperatureCurie temp°CKono, Masaru
4TypeTypeKono, MasaruOptical microscopyType of thermomagnetic curve: NO, no oxidation, HT, high-temperature oxidation, LT, low-temperature oxidation
5StageStageKono, MasaruOptical microscopyOxidation stage = degree of high-temperature oxidation of titanomagnetite: N, L, M, H = no, low, moderate, high oxidation
6IlmeniteIlmKono, MasaruOptical microscopyPresence of ilmenite lamellae in (III) planes of (titano-) magnetite host crystal
7PseudobrookitePsbKono, MasaruOptical microscopyPresence of pseudobrookite as oxidation product of Ti-rich phase
8TitanomagnetiteTimagKono, MasaruOptical microscopyPresence of low-temperature oxidation product
9CommentCommentKono, Masaru
Size:
97 data points