Fujioka, Kantaro (1980): (Table 1) Geochemistry of hornblende phenocryst at DSDP Hole 57-439 [dataset]. PANGAEA, https://doi.org/10.1594/PANGAEA.822286, In supplement to: Fujioka, K (1980): Conglomerates of volcanic rocks of Deep Sea Drilling Project Site. In: Scientific Party, Initial Reports of the Deep Sea Drilling Project, 56/57 (eds.), Initial Reports of the Deep Sea Drilling Project (U.S. Govt. Printing Office), 56-57, 1075-1082, https://doi.org/10.2973/dsdp.proc.5657.142.1980
Always quote citation above when using data! You can download the citation in several formats below.
Published: 1980 (exact date unknown) • DOI registered: 2013-12-16
Project(s):
Deep Sea Drilling Project (DSDP)
Coverage:
Latitude: 40.626800 * Longitude: 143.310500
Date/Time Start: 1977-11-03T00:00:00 * Date/Time End: 1977-11-03T00:00:00
Minimum Elevation: -1656.0 m * Maximum Elevation: -1656.0 m
Event(s):
57-439 * Latitude: 40.626800 * Longitude: 143.310500 * Date/Time: 1977-11-03T00:00:00 * Elevation: -1656.0 m * Penetration: 1157.5 m * Recovery: 160 m * Location: North Pacific/TRENCH * Campaign: Leg57 * Basis: Glomar Challenger * Method/Device: Drilling/drill rig (DRILL) * Comment: 38 cores; 333.5 m cored; 0 m drilled; 48 % recovery
Parameter(s):
| # | Name | Short Name | Unit | Principal Investigator | Method/Device | Comment |
|---|---|---|---|---|---|---|
| 1 | Sample code/label | Sample label | Fujioka, Kantaro | DSDP/ODP/IODP sample designation | ||
| 2 | Silicon dioxide | SiO2 | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 3 | Titanium dioxide | TiO2 | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 4 | Aluminium oxide | Al2O3 | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 5 | Iron oxide, FeO | FeO | % | Fujioka, Kantaro | Electron microprobe (EMP) | Total iron |
| 6 | Manganese oxide | MnO | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 7 | Magnesium oxide | MgO | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 8 | Calcium oxide | CaO | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 9 | Sodium oxide | Na2O | % | Fujioka, Kantaro | Electron microprobe (EMP) | |
| 10 | Potassium oxide | K2O | % | Fujioka, Kantaro | Electron microprobe (EMP) |
License:
Creative Commons Attribution 3.0 Unported (CC-BY-3.0)
Size:
100 data points